Green Dragon Matt Glaze

Firing temperature : Cone 6 | Surface texture : matte | Color : turquoise green | Atmosphere: Oxidation/Neutral

Pictured here with blue Frasca Wood Ash Glaze over Green Dragon Matt.

Published in "Wood-Ash Glazing at Cone 6" by Harry Spring, in the Oct 2002 issue of Ceramics Monthly.