Firing temperature : Cone 6 | Surface texture : glossy | Color : golden yellow | Atmosphere: Oxidation/Neutral

Published in "Gemstones & Glazes" by Ryan Coppage, in the Sep 2017 issue of Ceramics Monthly.

 


Click Image to Enlarge
Download for Glaze Calculation
Hyperglaze |

Ingredients

Instructions

This item will be permanently deleted and cannot be recovered. Are you sure?

Once you submit this recipe for moderation you will no longer be able to edit its content.

Comments
  • Echlin D.

    This is a finicky glaze.It crazes on Laguna Bmix 5, and also pinholes. the color is nice, and it goes a little milky pink where it pools. I’d love this color in an opaque, satin finish,