Glossy #3

Firing temperature : cone 6-7 | Surface texture : glossy | Color : clear | Atmosphere: Oxidation/Neutral

Originally published in the May 2018 issue of Ceramics Monthly.


Click Image to Enlarge

Instructions

My favorite stain additions are Mason stain Bermuda, Mason stain Chartreuse, or Degussa Brilliant Orange stain.