Frasca Wood Ash Glaze

Frasca Wood Ash Glaze

Firing temperature : Cone 6 | Surface texture : matte | Color : medium blue | Atmosphere: Oxidation/Neutral

Pictured here over Green Dragon Matt Glaze.

Published in "Wood-Ash Glazing at Cone 6" by Harry Spring, in the Mar/Apr 2006 issue of Pottery Making Illustrated.


Click Image to Enlarge
Download for Glaze Calculation
Insight | Hyperglaze | Glaze Master

Ingredients

Instructions

For a green variation, add 4% copper carbonate; for blue, add 2% cobalt carbonate.