Ceramic Recipes logo

Flux Saturation (4-H4-O6)

Flux Saturation (4-H4-O6)

Firing temperature : Cone 6 | Surface texture : satin matte | Color : yellow | Atmosphere: Oxidation

Click Image to Enlarge

Instructions

This glaze is not food safe.

This recipe was sourced from The Ceramic Spectrum: A Simplified Approach to Glaze and Color Development by Robin Hopper.