Firing temperature : cone 5-6 | Surface texture : glossy | Color : green celadon | Atmosphere: Oxidation

This recipe was shared by Yoko Sekino-Bové in the December 2018 issue of Ceramics Monthly.


Click Image to Enlarge

Instructions

You can use any soda feldspar you have and and Gerstley Borate substitute, but always test first.