Eva’s Matte Off-White

Eva's Matte Off-White

Firing temperature : cone 5-6 | Surface texture : matte | Color : off white | Atmosphere: Oxidation

Click Image to Enlarge

Instructions

This is an off-white breaking glaze that ceramic artist Eva Champagne shared with me, although she doesn’t remember its origins. It is easy to work with. I use a thin application and mostly apply by dipping or pouring. The glaze interacts wonderfully with line carving and with the clay I use, Red Star, a stoneware made by Alligator Clay Company in Baton Rouge, Louisiana. I fire this glaze to cone 5 with a hold.

This recipe was shared by Osa Atoe in the September 2020 issue of Ceramics Monthly.

This item will be permanently deleted and cannot be recovered. Are you sure?

Once you submit this recipe for moderation you will no longer be able to edit its content.

Comments

Leave a Reply

You must be logged in to post a comment.

Enter Your Log In Credentials
This setting should only be used on your home or work computer.

Larger version of the image
Send this to a friend