Emerald

Emerald

Firing temperature : Cone 6 | Surface texture : glossy | Color : emerald | Atmosphere: Oxidation/Neutral

Published in "Gemstones & Glazes" by Ryan Coppage, in the Sep 2017 issue of Ceramics Monthly.

This is a fluid glaze that runs if thick, but does not craze.