Firing temperature : Cone 6 | Surface texture : satin | Color : various | Atmosphere: Oxidation/Neutral

This recipe was published in the May/June 2018 issue of Pottery Making Illustrated. This glaze originally came from Eric Mirabito. The surface is responsive to rates of cooling in the kiln.


Click Image to Enlarge

Instructions

Cool slowly for a true satin-matte surface. Fast cooling will show the glossier side of this glaze.