Firing temperature : Cone 6 | Surface texture : satin | Color : clear | Atmosphere: Oxidation

Click Image to Enlarge

Ingredients

Instructions

I apply this glaze by spraying, then cool the kiln slowly at the end of the firing to achieve a satin surface. Original recipe attributed to Eric Mirabito, shared with me by Chandra DeBuse.

This glaze was shared by Stephanie Wilhelm in the November 2019 issue of Ceramics Monthly.