Firing temperature : Cone 2–3 | Surface texture : glossy | Color : clear | Atmosphere: Oxidation

Click Image to Enlarge

Ingredients

Instructions

This is a glossy base that works well with ceramic stains and coloring oxides. Substitute all or part of the wollastonite with dolomite to create a satin to satin-matte surface.

This recipe was shared by Marc Egan in the September/October 2020 issue of Pottery Making Illustrated.