Ceramic Recipes logo

Edgy Green

Edgy Green

Firing temperature : Cone 6 | Surface texture : satin matte | Color : turquoise green | Atmosphere: Oxidation/Neutral

Published in "Electric Kiln Success" by Jonathan Kaplan, in the Jan/Feb 2008 issue of Pottery Making Illustrated.


Click Image to Enlarge
Download for Glaze Calculation
Insight | Hyperglaze | Glaze Master

Ingredients