Easy E Clear

Firing temperature : Cone 6 | Surface texture : glossy | Color : clear | Atmosphere: Oxidation/Neutral

This glaze is from John Britt’s book The Complete Guide to Mid‑Range Glazes.

Published in the May 2018 issue of Ceramics Monthly.


Click Image to Enlarge

Instructions

For best results, I spray a thin layer. This glaze also takes stain very well.