Firing temperature : cone 4-6 | Surface texture : satin | Color : blue | Atmosphere: Oxidation

Click Image to Enlarge

Instructions

Specific gravity: 1.43. A smooth and slightly fat matte surface. This glaze contains both magnesium oxide, which yields pastels, as well as barium oxide, which can make vivid colors. Adding cobalt carbonate in increments from 0.25–2% yields pale to strong lavenders, and adding 1% copper carbonate produces a bright turquoise. The surface becomes extremely dry and grainy with additions of 4% titanium dioxide and above.

Original recipe shared by Milt Friedly in the November 1991 issue of Ceramics Monthly. Not for functional ware.

This recipe was shared by Alisa Clausen in the February 2020 issue of Ceramics Monthly.

This item will be permanently deleted and cannot be recovered. Are you sure?

Once you submit this recipe for moderation you will no longer be able to edit its content.

Comments

Leave a Reply

You must be logged in to post a comment.

Enter Your Log In Credentials
This setting should only be used on your home or work computer.

Larger version of the image
Send this to a friend