Firing temperature : Cone 6 | Surface texture : satin | Color : white | Atmosphere: OxidationIngredients
- 14.73
Custer Feldspar (sub. Forshammer)
46.90- 8.34
- 30.03
- 4.33
- 4.33
- 8.24
- 3.25
Add:
Instructions
Specific gravity: 1.43. This glaze is opaque and glossy, but has a soft sheen on the surface. Many color variations were possible, all of which are opaque, bright, and clean. For color variations, omit the tin oxide, titanium dioxide, and zinc oxide. I substituted Forshammer feldspar for Custer feldspar.
Original recipe shared by Gerald Brown in the June 1991 issue of Ceramics Monthly.