The added Veegum T makes this glaze very brushable, which is often my preference.

I use D-Base glaze on the exterior of all my pots.

This glaze is fired to cone 8 in oxidation, but can be fired from con 6–8. It works best when applied thin, about the consistency of 1% milk. I always sieve and mix thoroughly before applying.

This glaze was shared by Doug Peltzman in the December 2019 issue of Ceramics Monthly.