Firing temperature : cone 4-6 | Surface texture : satin | Color : blue | Atmosphere: Oxidation

Click Image to Enlarge

Instructions

Specific gravity: 1.43. A calcium matte with a hard and flat surface. The color tests showed a neutral color response; however, the red iron oxide showed some variegation with yellows on a rust ground. I substituted Forshammer feldspar for Custer feldspar.

From Pottery Making Illustrated.

This recipe was shared by Alisa Clausen in the February 2020 issue of Ceramics Monthly.