Firing temperature : cone 4-6 | Surface texture : glossy | Color : clear | Atmosphere: Oxidation

Click Image to Enlarge

Instructions

This is a good all-around, stable glaze that can be applied via dipping, brushing, or pouring. Mix to the consistency of 2% milk.

This recipe was shared by Naomi Clement in the November/December 2019 issue of Pottery Making Illustrated.

 