Chris Wolff’s Cream Gloss Glaze

Chris Wolff’s Cream Gloss Glaze

Firing temperature : Cone 6 | Surface texture : glossy | Color : cream | Atmosphere: Oxidation/Neutral

Soft cream beneath a very glossy shell; works well over the plum glaze.

Published in "School and Beyond" by Andy Cantrell, in the May 2000 issue of Ceramics Monthly.