Ceramic Recipes logo

Charcoal Satin Matt Glaze

Charcoal Satin Matt Glaze

Firing temperature : Cone 6 | Surface texture : satin matte | Color : gray | Atmosphere: Oxidation/Neutral

Published in "Making Stable Glazes for Functional Stoneware and Porcelain" by John Hesselberth and Ron Roy, in the Sept 2000 issue of Ceramics Monthly.

 

 


Click Image to Enlarge
Download for Glaze Calculation
Insight | Hyperglaze | Glaze Master

Ingredients

Instructions

Cool slowly or it will turn glossy.