Firing temperature : Cone 6 | Surface texture : glossy | Color : clear | Atmosphere: Oxidation

Click Image to Enlarge

Instructions

I use this as a clear glaze and as a base glaze with added colorants. This recipe was developed by Jeff Campana. Found in The Complete Guide to Mid-Range Glazes by John Britt, Sterling Publishing, 2014.

This recipe was shared by Jackie Head in the March 2019 issue of Ceramics Monthly.