Bristol Glaze IX
Firing temperature : Cone 6 | Surface texture : matte | Color : light green | Atmosphere: Oxidation/NeutralPublished in "Bristol Glazes" by Cheryl Pannabecker, in the Mar/Apr 2011 issue of Pottery Making Illustrated.
Ingredients
- 8.7
- 9.3
- 25.9
- 9.7
- 11.3
- 35.1
Instructions
I used calcined zinc - as recommended in Glaze Projects and Ferro Frit 3269 to replace Pemco Frit 25. Glazes were tested on Standard Ceramic Clay bodies; Brooklyn Red and Buff Clay, bisqued to cone 05.