Bright Clear

Firing temperature : Cone 6 | Surface texture : glossy | Color : clear | Atmosphere: Oxidation/Neutral Reduction

This is a glaze I got from my time at NSCAD in Nova Scotia. It's a great cone 6 base, and applies really nicely (you can both brush and dip it with equal success). It also takes colorants well.

Published in "Emerging Artist Recipes" in the May 2017 issue of Ceramics Monthly.