Bob’s Altered – SiC CoO

Bob’s Altered – SiC CoO

Firing temperature : Cone 6 | Surface texture : textured | Color : black | Atmosphere: Oxidation/Neutral

Published in "Silicon Carbide: The Stuff of Stars" by Mark Chatterley, in the March 2011 issue of Ceramics Monthly.

This glaze is not food safe.


Click Image to Enlarge
Download for Glaze Calculation