Firing temperature : Cone 6 | Surface texture : matte | Color : black | Atmosphere: OxidationIngredients
- 1
- 1
(In Parts):
Instructions
I paint this wash onto bisque-fired Hopeful Birds then wipe off the excess so it remains in textured areas. Next, I apply Amaco Velvet underglazes, blending and applying in various thicknesses.
This recipe was shared by Rita Vali in the January 2021 issue of Ceramics Monthly.