Firing temperature : Cone 6 | Color : various | Atmosphere: Oxidation/Neutral Reduction

Published in the March 2018 issue of Ceramics Monthly.

This recipe is from John Britt’s book, The Complete Guide to Mid-Range Glazes. The recipe was altered with progressive additions of cobalt oxide, rutile, and ash