Instructions

I use this glaze often in my work and find that it's very reliable. It's a variation of Plainsman Clays' published come 6 Ravenscrag Clear glaze. For more color options, make tests that alter the percentages or types of colorants used.

This recipe was shared by Dawn Candy in the May 2019 issue of Ceramics Monthly.