Ceramic Recipes logo

AC GG Base

AC GG Base

Firing temperature : Cone 6 | Surface texture : satin matte | Color : gray | Atmosphere: Oxidation

Click Image to Enlarge

Ingredients

Instructions

A simple strontium base, which can be colored with stains or oxides. A crater surface can be achieved with the addition of 2–5% magnesium carbonate. Shown with 5 and 10% titanium dioxide.

This recipe was shared by Alisa Liskin Clausen in the May 2019 issue of Ceramics Monthly.