520 Shiny Clear Glaze

520 Shiny Clear Glaze

Firing temperature : Cone 6 | Surface texture : glossy | Color : clear | Atmosphere: Oxidation

Click Image to Enlarge

Instructions

Mix to table cream consistency. This is a forgiving glaze with a wide working range of specific gravity and application thickness. It accepts Mason stains from 5–15%. Add 10% Mason stain 6236 Chartreuse for a bright green (see bowl interior).

This recipe was shared by Rita Vali in the January 2021 issue of Ceramics Monthly.