20x5 Ash Clear
Firing temperature : cone 7 | Surface texture : glossy to satin | Color : clear | Atmosphere: Oxidation ReductionIngredients
- 20
- 20
- 20
- 20
- 20
Instructions
When testing feldspars, try using Cuter Feldspar first. This glaze should be mixed very thin, to a specific gravity of 1.32.
This recipe was shared by Nathan Willever in the May 2019 issue of Ceramics Monthly.