Firing temperature : cone 04-03 | Surface texture : glossy | Color : green | Atmosphere: Oxidation

Click Image to Enlarge

Instructions

This glaze is runny when fired. I apply thickly, like Elmer's glue consistency, high on the pot so it can drip. Firing to cone 04 is ideal. The color shifts to olive green when fired to cone 03.

This recipe was shared by Lisa Orr in the November 2019 issue of Ceramics Monthly.