Ron Myers Clear
Firing temperature : cone 04-6 | Surface texture : glossy | Color : clear | Atmosphere: OxidationIngredients
- 80
- 10
- 10
- 10
Add:
Instructions
I used Mason stain #6025 Coral Red as the colorant in the process images.
This recipe was shared by Alan Johnson in the January/February 2021 issue of Pottery Making Illustrated.