Pete Pinnell's Terra Sigillata
Firing temperature : cone 06 | Surface texture : matte to satin | Color : black | Atmosphere: Raku ReductionIngredients
- 10.0
Instructions
I make terra sigillata in much smaller batches so I mix up ¹/5 of this recipe, which fits in a 1-gallon jar. The clay body I use is Continental Clay’s raku body.
This recipe was shared by Andy Bissonnette in the March 2021 issue of Ceramics Monthly.