Peeling Paint

Peeling Paint

Firing temperature : cone 08-01 | Surface texture : textured | Color : medium brown | Atmosphere: Oxidation/Neutral

Published in "Lee Akins" by Rafael Molina-Rodriquez, in the Aug/Sep 2006 issue of Ceramics Monthly.


Click Image to Enlarge
Download for Glaze Calculation
Insight | Hyperglaze | Glaze Master

Ingredients

Instructions

For Green: add 3–5% copper carbonate

For Blue: add 3% Cobalt Carbonate

For Black: add 5% Cobalt Carbonate, 5% Red Iron Oxide, 10% Black Stain