Metallic Platinum

Firing temperature : cone 05 | Surface texture : glossy | Color : metallic | Atmosphere: Oxidation/Neutral

Metallic Platinum can been seen on the raised bumps in the image shown on this page.

Published in "Studio Takada" by Kaname and Sumiko Takada, in the March 2017 issue of Ceramics Monthly.


Click Image to Enlarge
Download for Glaze Calculation
Insight | Hyperglaze | Glaze Master

Ingredients

Instructions

This glaze shifts slightly at cone 05.