Firing temperature : cone 2–5 | Surface texture : glossy | Color : clear | Atmosphere: Oxidation Reduction

Click Image to Enlarge

Instructions

Mix the glaze to a whole-milk consistency. The thinnest possible layer is recommended for most low-fire clear glazes; however, a standard 3-second count application of this glaze works best. It takes colorants well and works over underglazes and terra sigillatas.

This recipe was shared by Marty Fielding in the in the December 2020 issue of Ceramics Monthly.