Ceramic Recipes logo

Matt Kelleher Gloss–Opaque Butter Yellow

Matt Kelleher Gloss–Opaque Butter Yellow

Firing temperature : cone 3 | Surface texture : glossy | Atmosphere: Oxidation/Neutral

Published in "Low-fire to cone 3 Recipes," in the September 2018 issue of Ceramics Monthly.

The image shown here has multiple glazes on it. This is the first color addition.


Click Image to Enlarge

Ingredients

Instructions

I use this as a liner glaze. Apply thinly for clear. For opaque colors, mix to a heavy-cream consistency for a thicker application.