Low Fire Crackle

Firing temperature : cone 04 | Surface texture : glossy | Color : blue | Atmosphere: Oxidation

Click Image to Enlarge

Ingredients

Instructions

Brush 3–5 even coats onto work. Fire to cone 04. Glaze can be very runny depending on thickness and hold at top temperature. Because this glaze can gel, I add a couple of drops of Darvan and only mix it in small batches.

This recipe was shared by Mike Gesiakowski in the July/August 2019 issue of Pottery Making Illustrated.