Lok Ming Fung Copper-Iron Green Glaze for Earthenware

Lok Ming Fung Copper-Iron Green Glaze for Earthenware

Firing temperature : cone 04 | Surface texture : matte | Color : medium green | Atmosphere: Oxidation/Neutral

Published in "Cool Colors" by Linda Bloomfield, in the Feb 2012 issue of Ceramics Monthly.


Click Image to Enlarge
Download for Glaze Calculation
Insight | Hyperglaze | Glaze Master

Ingredients

Instructions

Glaze runs when applied thickly.

The author uses Ferro Frit 3110 when high alkaline frit is listed in a recipe. She notes that the frit sometimes causes glazes to craze. To correct this, try substituting a higher boron frit.

This item will be permanently deleted and cannot be recovered. Are you sure?

Once you submit this recipe for moderation you will no longer be able to edit its content.

Comments

Leave a Reply

You must be logged in to post a comment.

Enter Your Log In Credentials
This setting should only be used on your home or work computer.

Larger version of the image
Send this to a friend