Lichen Glaze

Lichen Glaze

Firing temperature : cone 04-6 | Surface texture : textured | Color : various | Atmosphere: Oxidation/Neutral Reduction

This recipe is not food safe. This recipe is nice in Raku. Nice over shiny glazes. Crawly, beaded surface. Shown in the image here on top of a blue terra sigillata and Faux Lead Hulk Smash  glaze and Faux Lead Amber.

Published in "Low-Fire Surfaces" by Ronan Kyle Peterson, in the September 2017 issue of Ceramics Monthly.


Click Image to Enlarge

Instructions

Works best layered over Faux Lead glaze. It's dry, flaky, and sharp when used by itself.