Lana Wilson Purple Aqua
Firing temperature : cone 06 | Surface texture : textured | Color : medium purple | Atmosphere: Oxidation/NeutralVery dry matt but smooth. thickness strongly affects color. Best results when thick and thin...shows a lot of variation. LW recipe says purple where thin and aqua where thick. I have found just the opposite. From Ceramics Monthly, June 1995 and other published sources.
Ingredients
- 48
- 48
- 4
- 2
Additions
Instructions
copper carb from 4 to 8 %