Firing temperature : cone 3 | Surface texture : satin | Color : clear | Atmosphere: Oxidation/Neutral

Published in "Low-fire to cone 3 Recipes," in the September 2018 issue of Ceramics Monthly.

The image shown here has multiple glazes on it.


Click Image to Enlarge

Ingredients

Instructions

This recipe has been recalculated from the original to fire to cone 3. Apply very thinly for the best transparency. I control the cooling of the kiln at a rate of 100° an hour between 1900° and 1400°F for the best satin surface. Natural cooling produces a bit more gloss.