Kelley’s Low-Fire Shino

Kelley’s Low-Fire Shino

Surface texture : matte | Color : medium tan | Atmosphere: Raku

Published in "Beyond the Norm: Experimenting with "Alternative" Raku Glazes" by Steven Branfman, in the Jul/Aug 2007 issue of Pottery Making Illustrated.


Click Image to Enlarge
Download for Glaze Calculation
Insight | Hyperglaze | Glaze Master

Ingredients

Instructions

This is a semi-opaque glaze with excellent crackle and lovely tan to silvery color characteristics and texture depending on firing temp. Works well in combination with other glazes.