Ceramic Recipes logo

Kat Red

Kat Red

Firing temperature : cone 04 | Surface texture : satin matte | Color : dark red | Atmosphere: Oxidation/Neutral

Published in "Deep Plates" by Kristin Pavelka, in the Sep/Oct 2011 issue of Pottery Making Illustrated.


Click Image to Enlarge
Download for Glaze Calculation
Insight | Hyperglaze | Glaze Master

Ingredients

Instructions

This is an opaque, fat-looking satin glaze.

This item will be permanently deleted and cannot be recovered. Are you sure?

Once you submit this recipe for moderation you will no longer be able to edit its content.

Comments

Leave a Reply

You must be logged in to post a comment.

Enter Your Log In Credentials
This setting should only be used on your home or work computer.

Larger version of the image
Send this to a friend