Firing temperature : cone 04 | Surface texture : satin matte | Color : light green | Atmosphere: Oxidation/Neutral

This glaze is not safe for surfaces that come into contact with food.

Published in "Polychrome Glazes" by Joan Bruneau, in the April 2014 issue of Ceramics Monthly.


Click Image to Enlarge
Download for Glaze Calculation
Insight | Hyperglaze | Glaze Master

Ingredients

Instructions

Add 5-10% whiting along with stains that need the presence of calcium to enhance color, ie: Victoria Green Mason stain, Chartreuse Mason stain, or chrome-tin pinks.

This item will be permanently deleted and cannot be recovered. Are you sure?

Once you submit this recipe for moderation you will no longer be able to edit its content.

Comments

Leave a Reply

You must be logged in to post a comment.

Enter Your Log In Credentials
This setting should only be used on your home or work computer.

Larger version of the image

Send this to a friend