Icy Blue Glaze

Firing temperature : cone 04 | Surface texture : satin matte | Color : turquoise blue | Atmosphere: Oxidation/Neutral

Recipe adapted by Kari Radasch from a Wood Hughes recipe.

Published in "Cake? Just Add Flower!" by Arthur Halvorsen, in the Nov/Dec 2010 issue of Pottery Making Illustrated.


Click Image to Enlarge

Instructions

This glaze works best when it is not too thick. If the glaze application is thicker than normal (more than the thickness of a dime) it runs excessively.