Glaze 5
Firing temperature : cone 04 | Surface texture : textured | Color : various | Atmosphere: Oxidation/Neutral ReductionThis recipe was originally published in the January/February 2018 issue of Pottery Making Illustrated.
Ingredients
- 25
- 33
- 33
- 2
- 7
Add:
Instructions
The crawl/crackle pattern is tighter, more satiny, and less spaced out, more like a gradual stretching and splitting. On the low-fire white clay body, the pattern is more distinct, drier, and more crackled. Not food safe.