Firing temperature : cone 04 | Surface texture : textured | Color : various | Atmosphere: Oxidation/Neutral Reduction

This recipe was originally published in the January/February 2018 issue of Pottery Making Illustrated.


Click Image to Enlarge

Instructions

The fit of this glaze is tight, with no peeling up. The pattern is interesting, random, and the glaze is very hard. There is a small bit of sparkle. Not food safe.