Glaze 3
Firing temperature : cone 04 | Surface texture : textured | Color : blue | Atmosphere: Oxidation/Neutral ReductionThis recipe was originally published in the January/February 2018 issue of Pottery Making Illustrated.
Ingredients
- 50
- 20
- 20
- 10
Add:
Instructions
Sandy, scratchy, rough like a nail file. This glaze takes color well and has an incredibly dry, matte surface. Not food safe.
This item will be permanently deleted and cannot be recovered. Are you sure?
Once you submit this recipe for moderation you will no longer be able to edit its content.
Comments