Glaze 2
Firing temperature : cone 04 | Surface texture : textured | Color : green | Atmosphere: Oxidation/Neutral ReductionThis recipe was originally published in the January/February 2018 issue of Pottery Making Illustrated.
Ingredients
- 80
- 20
Add:
Instructions
This glaze with the addition of titanium makes a lustrous satin glaze. Both Little Loafers and white earthenware clay bodies handled this glaze well. The color of the stain shifted from blue to light copper green. Not food safe.
This item will be permanently deleted and cannot be recovered. Are you sure?